Grade :
|
403S17 耐腐蚀钢片/板和带材
|
|
|
|
|
|
Number:
|
X6Cr13
|
|
|
|
|
|
Classification:
|
铁素体不锈钢
|
|
|
|
|
|
Density:
|
7.7 g/cm ³
|
|
|
|
|
|
Standard:
|
EN 10088-2:2005不锈钢。通用耐腐蚀钢片/板和带材交货技术条件
|
|
|
|
|
|
EN 10088-3:2005不锈钢。一般用途耐腐蚀钢的半成品、棒材、线材、型材和光亮产品的交货技术条件
|
|
|
|
|
|
EN 10088-1:2005不锈钢。不锈钢清单
|
|
|
|
|
|
|
|
|
|
|
|
Equivalent grades:
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Chemical comb % of steel X6Cr13 (403S17 ): EN 10088-2-2005
|
|
|
|
|
|
|
未经买方同意,不得故意将本表中未列出的元素添加到钢材中,除非对铸件进行精加工。
|
|
|
|
|
|
|
特定的硫含量范围可以改善特定的财产。对于可加工性,建议并允许将硫含量控制在0.015%至0.030%之间。对于可焊性,建议并允许将硫含量控制在0.008%至0.030%之间。对于可极化性,建议将硫含量控制在最大0.015%。
|
|
|
|
|
|
|
|
|
|
|
|
|
|
C
|
Si
|
Mn
|
P
|
S
|
Cr
|
|
max 0.08
|
max 1
|
max 1
|
max 0.04
|
max 0.015
|
12月14日
|
|
|
|
|
|
|
|
|
Mechanical properties of steel X6Cr13 (403S17 )
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Rm - Tensile strength (MPa) (+A)
|
400-600
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Rp0.2 0.2% proof strength (MPa) (+A)
|
220-240
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
A - Min. elongation at fracture (%) (+A)
|
19
|
|
|
|
|
|
|
|
|
|
|
|
|
Brinell hardness (HB): (+A)
|
200
|
|
|
|
|
|
|
|
|
|
|
|
|
Properties of steel X6Cr13 (403S17 )
|
|
|
|
|
|
|
Resistance to intergranular corrosion: in the delivery condition - no; in the welded condition - no
|
|
|
|
|
|
|
|
|
|
|
|
|